Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 190 - 218 °C | 374 - 425 °F | Average value: 207 °C Grade Count:62 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 - 218 °C | 140 - 425 °F | Average value: 199 °C Grade Count:130 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.4 - 218 °C | 175 - 424 °F | Average value: 192 °C Grade Count:18 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |