Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 170 - 213 °C | 338 - 415 °F | Average value: 196 °C Grade Count:3 |
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 204 - 213 °C | 400 - 415 °F | Average value: 208 °C Grade Count:13 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 - 213 °C | 158 - 415 °F | Average value: 193 °C Grade Count:78 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 204 - 213 °C | 400 - 415 °F | Average value: 208 °C Grade Count:8 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 - 213 °C | 158 - 415 °F | Average value: 173 °C Grade Count:4 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 - 213 °C | 145 - 415 °F | Average value: 136 °C Grade Count:47 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |