Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 89.0 - 177 °C | 192 - 350 °F | Average value: 149 °C Grade Count:38 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 175 - 177 °C | 347 - 350 °F | Average value: 176 °C Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 - 177 °C | 310 - 351 °F | Average value: 166 °C Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 130 - 177 °C | 266 - 351 °F | Average value: 162 °C Grade Count:31 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |