Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 128 °C
140 - 262 °F
Average value: 78.0 °C Grade Count:18
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..