Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 101 °C
100 - 214 °F
Average value: 67.4 °C Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Deflection Temperature at 1.8 MPa (264 psi) 52.0 - 101 °C
126 - 214 °F
Average value: 67.8 °C Grade Count:4
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..