Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Plaskolite Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Plaskolite West Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Resirene Resirene® HH-103 General Purpose Polystyrene Features:Low FlowHigh HeatHigh Molecular WeightMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:ExtrusionFoamGPPS/HIPS BlendsInformation provided by US distributor Calsak Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.35 mm |
196 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
LG Chemical LI-943 ASA Resin
(discontinued **) Heat resistance, Excellent weather resistance, Well balanced mechanical properties, Superior chemical resistance, Good thermal aging stability, Good moldability and processability, Applications incl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75A |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1,-2 |
Ineos ABS Lustran® ABS 650 Injection Molding Grade Lustran® ABS 650 has high impact strength, high flow, and is injection molding grade. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS (Asia Pacific) LNP* Thermocomp* CX05470 is a compound based on Polystyrene resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | 0.5 inch; ASTM D648 |
PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1,-2 |
Covestro Bayblend® FR3100 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers with very low .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
A. Schulman ComAlloy Voloy® 411 Mineral Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75 -1 & -2 flat |
Asahi Kasei Tenac®-C 4563 Copolymer Acetal Resin Weather-Resistant grade containing UV absorber and other additives for superior weathering abilityInformation provided by Asahi Kasei Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Beijing Chemical Industry KAIFA® GL5100 ABS Extrusion Grade Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Plaskolite West Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |