Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C @Thickness 3.18 mm |
160 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2798 Polyvinyl Chloride, Rigid (PVC, Rigid) Premium chemical resistant Compound for Packaging.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C @Thickness 3.18 mm |
160 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C @Thickness 3.18 mm |
160 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C @Thickness 6.35 mm |
160 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings 210A White 271(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 - 249 °C | 160 - 480 °F | Average value: 174 °C Grade Count:14 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0177 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6 M L Nylon 66 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Fast Molding Cycle, Low Viscosity and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6 Nylon 66 Availability: North AmericaForms: PelletsFeatures: Low ViscosityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Chase Plastics CP Pryme® N100HSL (COND, 50% RH) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Chase Plastics CP Pryme® N100MD2 (COND, 50% RH) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Chase Plastics CP Pryme® N300L (COND, 50% RH) Nylon 6 (Utility Grade), Internally Lubricant Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Chase Plastics CP Pryme® N300L (DAM) Nylon 6 (Utility Grade), Internally Lubricant Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static) Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D-648 |
Axiall 7555 Rigid PVC, Extrusion, Natural Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D-648 |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | ASTM D648 |
Asahi Kasei Thermofil P-9900-0576 Unreinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 FR 344 BK Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C | 160 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PBT 0166 B FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |