Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 65.56 °C | 150.0 °F | ASTM D648 |
Lucent Polymers CPP-230 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.56 °C | 150.0 °F | ASTM D648 |
Lucent Polymers CPP-240 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.56 °C | 150.0 °F | ASTM D648 |
Lucent Polymers PBT-310 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |