Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products FT5100-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Nylene® Vexel™ B50U , High Flow, Un-reinforced PBT Description: Vexel™ B50U is a high flow, un-reinforced PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 - 60.0 °C | 130 - 140 °F | Average value: 56.8 °C Grade Count:3 |
Overview of materials for Nylon 11 with Graphite Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA12 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Spartech EP5220 Calcium Carbonate Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0320 S1 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0475 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Chase Plastics CP Pryme® NN200STL (DAM) Nylon 66, Super-Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 - 141 °C | 130 - 285 °F | Average value: 97.3 °C Grade Count:29 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Chase Plastics CP Pryme® PPC100-8M Polypropylene Copolymer Information provided by Chase Plastics. |