Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Moplen HP400L Polypropylene Homopolymer Description: All ingredients in HP400L meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Toys, containers, lids, medical applications, closure capsInformation provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Moplen HP400N Polypropylene Homopolymer Description: HP400N is a high flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP400N is designed for injection molding a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Moplen HP550J Polypropylene Homopolymer Description: HP550J, a general purpose polypropylene homopolymer resin, is suitable for general extrusion and film fiber applications. HP550J resin meets FDA requirements in the Code of Federal Reg.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ CB267 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB267 medium melt flow, 1,600 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin has an excellent balance of scratch and mar resistance, rigidity and impac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for injection molded automotive interior applications.Availability: A.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ISO 75-2/A |
ExxonMobil PP7054L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | |
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | |
Aclo Accutech Polypropylene Copolymer CP0437C40L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | |
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | |
Aclo Accutech Polypropylene Copolymer CP0437W10L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ASTM D648 |
Cast Nylons Nycast® 12 Cast Nylon 12 NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | ISO 75-2/A |
ExxonMobil PP1364E2 Polypropylene Homopolymer Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C @Thickness 3.17 mm |
124 °F @Thickness 0.125 in |
Unannealed; ISO 75-2-92 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.1 °C | 124 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifax™ ETA3163/1 Thermoplastic Polyolefin Elastomer Description: Hifax™ ETA3163/1 medium melt flow, 900 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness and low temper.. |