Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | Unannealed; ASTM D648 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ CA244 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA244 high melt flow, 850 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, processability and dynamic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ CB251 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB251 medium melt flow, 1,200 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of impact resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | ASTM D648 |
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | ISO 75-2/A |
ExxonMobil Exxtral™ BNT 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.Availability: Africa & Middle East, Asia Pacific, E.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | ISO 75-2/Af |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | ISO 75-2/A |
ExxonMobil PP7033L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.2 °C | 117 °F | |
Aclo Accutech Polypropylene Copolymer CP0437C20L1 Calcium Reinforced |