Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 343 °C | 650 °F | Unannealed; ASTM D648 |
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 343 °C | 650 °F | Unannealed; ASTM D648 |
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 343 °C | 649 °F | ISO 75A-f |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 343 °C | 649 °F | ISO 75-f |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |