Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 328 °C | 622 °F | ISO 75-f |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 328 °C | 622 °F | ISO 75-f |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 328 °C | 622 °F | ISO 75-1/-2 |
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced PEEK-GF30Information provided by BARLOG plastics GmbH. |