Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | |
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | |
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | |
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | |
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C @Thickness 3.20 mm |
509 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | GB/T 1634.2-2004 |
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40 Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | ISO 75-1/-2 |
Barlog Plastics KEBATRON C2040G5 PPS, cross-linked, 40% GF, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | ISO 75-1/-2 |
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | ISO 75-1/-2 |
Barlog Plastics KEBATRON L2040G3 PPS, linear, 40% glass fiber reinforced, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |