Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 204.44 °C | 399.99 °F | ASTM D648 |
Lucent Polymers G6-33 Nylon 6, 33% Glass Fiber Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |