Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (DAM)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ISO 75A |
Lucite International Diakon® CMH454L Acrylic Polymer Information provided by Lucite International |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
Hannam Chemical Hanalac HU-600 ABS |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF/M30 CC BK 30% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 30% Filler by WeightFeatures: Chemically Coupled and CopolymerAppearance: BlackInformation provided by TP Composites, In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AF006XXZ ABS LNP* THERMOCOMP* AF006XXZ is a compound based on ABS resin containing 30% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM HO TL20 BN042 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® GA-4025 ABS, 25% Glass Filled Permanent static prevention material with 25% GF reinforcement that can be used in OA device and trayInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp PK0049 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0049 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific) LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | 0.5 inch unannealed; ASTM D648 |
PlastxWorld CEVIAN® SKG10 10% GF ABS Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ISO 75 |
Eurotec® Tecolen® CP30 GR20 NL PPCP, 20% glass fiber reinforced, natural, high flow grade Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
Beijing Chemical Industry KAIFA® M105N MPPO Resin High flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 216 °F | ASTM D648 |
Ashley Polymers Ashlene® PPO 263 A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer |