Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 101.0 °C | 213.8 °F | annealed; ASTM D-648 |
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101.0 °C | 213.8 °F | annealed; ASTM D-648 |
Axiall ProTherm® 4510 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4510 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high che.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 101.0 °C | 213.8 °F | annealed; ASTM D-648 |
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4526 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high res.. |