Thermal Properties | Metric | English | Comments |
---|---|---|---|
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Annealed Bar 0.5 - 1.23 in. dia ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Solution Treated Annealed Bar 0.5 - 1.23 in. dia ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded, Mill Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Beta Transus | 957 - 971 °C | 1750 - 1780 °F | |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |