Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® AS LF 20 PA66-Z20 Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15 Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® EBV-2H PA6-GF20 Product description: Grilon EBV-2H is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 20% glass fibers. Grilon EBV-2H has the following important properties: High melt streng.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20 Product description: Grivory GV-2 FWA natural is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-2H black PA*-GF20 Product description: Grivory GV-2H is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide. Grivory.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSS/4 LF 1 PA666 Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSS/4 LF 2 PA666 Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20 Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly.. |
|||
Deflection Temperature at 8.0 MPa | 65.0 °C | 149 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 5004 (BM-30/2 UV) PA666-MD30 Product description: Grilon XE 5004 is a normal viscosity PA6 injection molding grade with 30% mineral reinforcement, which is additionally UV stabilized. Grilon XE 5004 has the following important .. |