Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 178 °C | 352 °F | ISO 75 Cf |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |