Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40 Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35 Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-35/4 PA666-GF35 Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35 Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50 Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVX-5 H black 9915 PA*-GF50 Product description: Grivory GVX-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50 Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-2 |
Hexion Bakelite™ PF 7595 Phenolic Formaldehyde Resin, Low Coefficient of Friction, Galvanized, Conductive
(di Phenolic molding compound, inorganically/organically filled, modified with graphite, good heat conductivity, good sliding properties, conductive in electrical properties.Application areas: Bearers f.. |
|||
Deflection Temperature at 8.0 MPa | 175 °C | 347 °F | ISO 75-2 |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |