Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 825 °C @Thickness 0.800 mm |
1520 °F @Thickness 0.0315 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Glow Wire Test | 825 °C @Thickness 3.00 mm |
1520 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Glow Wire Test | 825 °C @Thickness 0.800 mm |
1520 °F @Thickness 0.0315 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Glow Wire Test | 825 °C @Thickness 1.00 mm |
1520 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Glow Wire Test | 825 °C @Thickness 2.50 mm |
1520 °F @Thickness 0.0984 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Glow Wire Test | 825 °C @Thickness 1.00 mm |
1520 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Glow Wire Test | 825 °C @Thickness 3.00 mm |
1520 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Glow Wire Test | 825 °C @Thickness 3.00 mm |
1520 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 18 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 18 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 27 U Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® FC 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® FC 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
Ignitability; IEC 60695-2-13 |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 825 °C @Thickness 0.710 mm |
1520 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Glow Wire Test | 825 °C @Thickness 3.00 mm |
1520 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Glow Wire Test | 825 °C @Thickness 1.50 mm |
1520 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 825 °C @Thickness 2.00 mm |
1520 °F @Thickness 0.0787 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
Glow Wire Test | 825 °C @Thickness 3.00 mm |
1520 °F @Thickness 0.118 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |