Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Glow Wire Test | 800 °C @Thickness 3.00 mm |
1470 °F @Thickness 0.118 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 0.800 mm |
1470 °F @Thickness 0.0315 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Glow Wire Test | 800 °C @Thickness 3.00 mm |
1470 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 1.00 mm |
1470 °F @Thickness 0.0394 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 19 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 24 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Diameter 3.00 mm |
1470 °F @Diameter 0.118 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 800 °C @Diameter 0.800 mm |
1470 °F @Diameter 0.0315 in |
GWFI; IEC 60695-2-12 |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Glow Wire Test | 800 °C @Diameter 3.00 mm |
1470 °F @Diameter 0.118 in |
GWFI; IEC 60695-2-12 |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
GWFI/GWT |
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Glow Wire Test | 800 °C @Thickness 40.6 mm |
1470 °F @Thickness 1.60 in |
Glow Wire Ignition Temp; DAM; IEC 60695-2-13 |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 800 °C @Thickness 1.00 mm |
1470 °F @Thickness 0.0394 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 800 °C @Thickness 0.800 mm |
1470 °F @Thickness 0.0315 in |
ALL, Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |