Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**) Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a.. |
|||
Glow Wire Test | 775 °C @Thickness 0.400 mm |
1430 °F @Thickness 0.0157 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Glow Wire Test | 775 °C @Thickness 1.60 mm |
1430 °F @Thickness 0.0630 in |
IEC 60695-2-13 |
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Glow Wire Test | 775 °C @Diameter 0.800 mm |
1430 °F @Diameter 0.0315 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Glow Wire Test | 775 °C @Diameter 0.400 mm |
1430 °F @Diameter 0.0157 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Diameter 1.50 mm |
1430 °F @Diameter 0.0591 in |
GWIT; IEC 60695-2-13 |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 3.20 mm |
1430 °F @Thickness 0.126 in |
Ignition Temperature; DAM; IEC 60695-2-13 |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Glow Wire Test | 775 °C @Thickness 38.1 mm |
1430 °F @Thickness 1.50 in |
GWIT; IEC 60695-13 |
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Akulon® XG-FKGS6 PA6-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free |
|||
Glow Wire Test | 775 °C @Thickness 0.900 mm |
1430 °F @Thickness 0.0354 in |
BK, Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 1.60 mm |
1430 °F @Thickness 0.0630 in |
Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecolen® CP30 NL XC30 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® MX 1004 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |