Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® C CM 206 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature, dry; IEC 60695-2-13 |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 700 °C @Thickness 0.750 mm |
1290 °F @Thickness 0.0295 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Glow Wire Test | 700 °C @Thickness 3.00 mm |
1290 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Glow Wire Test | 700 °C @Thickness 0.900 mm |
1290 °F @Thickness 0.0354 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Glow Wire Test | 700 °C @Thickness 1.50 mm |
1290 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Glow Wire Test | 700 °C @Thickness 0.710 mm |
1290 °F @Thickness 0.0280 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |