Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 600 °C @Thickness 2.00 mm |
1110 °F @Thickness 0.0787 in |
GWFI; IEC 60695-2-12 |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |