Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 3414R PC (Europe-Africa-Middle East) LEXAN 3414R is a high viscosity, 40% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 920A PC (Europe-Africa-Middle East) LEXAN 920A is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Glow Wire Test | 960 °C @Thickness 0.800 - 3.00 mm |
1760 °F @Thickness 0.0315 - 0.118 in |
Flammability Index; IEC 60695-2-12 |
PolyOne Bergamid™ A700 blue VN4817CF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 695-2-1 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East) LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 950 PC (Europe-Africa-Middle East) LEXAN 950 is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 18 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 24 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Diameter 0.400 mm |
1760 °F @Diameter 0.0157 in |
GWFI; IEC 60695-2-12 |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® FC 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI/GWT |
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
GWFI/GWT |
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
GWFI/GWT |
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
ISO 60695-2-12 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
ISO 60695-2-12 |
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America.. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
Glow Wire Flammability Index, dry; IEC 60695-2-12 |
DSM Akulon® XG-FKGS6 PA6-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
DAM; IEC 60695-2-1/2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
ALL, Glow-Wire Flammability; IEC 60695-2-12 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
ALL, Glow-Wire Flammability; IEC 60695-2-12 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR 30% Glass Reinforced, Flame Retardant (Halogen free) |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 695-2-1 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
GWFI/GWT |
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
Flammability Index; DAM; IEC 60695-2-12 |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |