Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 930 °C @Thickness 1.50 mm |
1710 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWIT; IEC 60695-2-13 |
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 930 °C @Thickness 1.00 mm |
1710 °F @Thickness 0.0394 in |
GWFI/GWT |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Glow Wire Test | 930 °C @Thickness 1.50 mm |
1710 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Glow Wire Test | 930 °C @Thickness 1.50 mm |
1710 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® FR 7087 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Glow Wire Test | 930 °C @Thickness 0.400 mm |
1710 °F @Thickness 0.0157 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Glow Wire Test | 930 °C @Thickness 0.400 mm |
1710 °F @Thickness 0.0157 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Glow Wire Test | 930 °C @Thickness 0.380 mm |
1710 °F @Thickness 0.0150 in |
Glow Wire Ignition Temperature, dry; IEC 60695-2-13 |
DSM Akulon® K225-KV PA6 FR(30) Flame Retardant (Halogen free), Heat stabilized |
|||
Glow Wire Test | 930 °C @Thickness 3.00 mm |
1710 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |