Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Glow Wire Test | >= 800 °C @Thickness 0.800 - 3.00 mm |
>= 1470 °F @Thickness 0.0315 - 0.118 in |
Flammability Index; IEC 60695-2-12 |
PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Glow Wire Test | 800 °C @Thickness 3.00 mm |
1470 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Glow Wire Test | 800 °C @Thickness 0.750 mm |
1470 °F @Thickness 0.0295 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 3.00 mm |
1470 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 18 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® 27 U Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Glow Wire Test | 800 °C @Thickness 1.00 mm |
1470 °F @Thickness 0.0394 in |
GWIT |
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Glow Wire Test | 800 °C @Thickness 0.800 mm |
1470 °F @Thickness 0.0315 in |
ignition temperature; ISO 60695-2-13 |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Glow Wire Test | 800 °C @Thickness 1.60 mm |
1470 °F @Thickness 0.0630 in |
ignition temperature; ISO 60695-2-13 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Glow Wire Test | 800 °C @Thickness 40.6 mm |
1470 °F @Thickness 1.60 in |
Glow Wire Ignition Temp; DAM; IEC 60695-2-13 |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 800 °C @Thickness 1.00 mm |
1470 °F @Thickness 0.0394 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Glow Wire Test | 800 °C @Thickness 0.750 mm |
1470 °F @Thickness 0.0295 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 800 °C @Thickness 2.00 mm |
1470 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NB40 GR20 NL XA70 PA6, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 800 °C @Thickness 1.50 mm |
1470 °F @Thickness 0.0591 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Glow Wire Test | 800 °C @Thickness 0.710 mm |
1470 °F @Thickness 0.0280 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Glow Wire Test | 800 °C @Thickness 3.00 mm |
1470 °F @Thickness 0.118 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |