Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Ignition Temperature; IEC 60695-2-13 |
PolyOne Bergamid™ A70 G25 U-SO TM Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 775 °C @Thickness 0.400 mm |
1430 °F @Thickness 0.0157 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Glow Wire Test | 775 °C @Diameter 0.800 mm |
1430 °F @Diameter 0.0315 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Diameter 0.750 mm |
1430 °F @Diameter 0.0295 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Glow Wire Test | 775 °C @Thickness 1.60 mm |
1430 °F @Thickness 0.0630 in |
GWIT; IEC 60695-2-12 |
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Diameter 3.00 mm |
1430 °F @Diameter 0.118 in |
GWIT; IEC 60695-2-13 |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Later 4-V0HF1 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
ignition temperature; ISO 60695-2-13 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Glow Wire Test | 775 °C @Thickness 0.400 mm |
1430 °F @Thickness 0.0157 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
DAM; IEC 60695-2-1/3 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecolen® CP30 NL XC30 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |