Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the .. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® H&T LGH 138 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 138 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, slip agent, antiblocking and processing aid, suitable for blown film extrusion.Films obtai.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the .. |
|||
Brittleness Temperature | >= -70.0 °C | >= -94.0 °F | ASTM D746 |
ExxonMobil LL 6235.19 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, Good Stiffness, Good ImpactUses: Food containers, Housewares, Toys |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 58D HDPE Blow Molding Resin
(discontinued **) Features: Good ESCR, high stiffness, good impact strength, slightly tougher alternative to Sclair 58A.Applications: Small part blow molding, food, pharmaceuticals, HIC containers.Data provided by th.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 2712 HDPE Injection Molding Resin Features: Good stiffness and impact resistance, minimal warpage, good top loading capability, high surface gloss.Applications: Aerosol overcaps, food containers, frozen food containers, seedling tra.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D 746 |
NOVA Chemicals Sclair® 2906 HDPE Injection Molding Resin NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Excellent toughness and impact resistance, High stiffness, Excellent processing stability, High GlossAdditives: .. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Micropol Microlin ML91 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Micropol Microstat ML21 Linear medium density static dissipative polyethylene Information provided by Micropol Limited |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D746 |
Lushan L-5R (HC) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Borealis Borecene™ RM8343PL Linear Polyethylene for Rotational Molding Borecene RM8343PL is plasma treated linear medium density natural polyethylene for rotational molding with improved adhesion properties. The material is plasma treated to change the chemical struct.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Borealis Borecene™ RM8403 Linear Polyethylene for Rotational Molding Borecene RM8403 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol Estane® 58201 Thermoplastic Polyurethane Type: Estane® 58201 is an 82A Polyether-type thermoplastic polyurethane (TPU) compound.Features: Tear resistant properties.Uses: Injection Molding and general extrusion techniques.Available in Euro.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer unmatched toughness and d.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
Chengdu Polyster H3303B Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and extrusion grade. Contains color-stable antioxidants. Excellent low-temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ boots, hose jack.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ISO 974 |
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE) Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | Compression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746 |
Dow DGDA-2475 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Ashley Polymers Ashlene® 935-40M Nylon 11 A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® RL 50 U Linear Medium Density Polyethylene Clearflex RL 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® T5083 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |