Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | Low temp embrittlement; ASTM D746 |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | Low temp embrittlement; ASTM D746 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | Low temp embrittlement; ASTM D746 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Brittleness Temperature | <= -51.0 °C | <= -59.8 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Teknor Apex APEX® 121 Polyvinyl Chloride, Flexible Notes: 90°C Jacket; RoHS Compliant Features: Good UV Resistance Uses: Telephone Drop Wire Insulation; Telephone Drop Wire JacketingAgency Ratings: REA Unspecified Rating Forms: PelletsInformation.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Teknor Apex Flexalloy® 9800-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Teknor Apex Flexalloy® 9800-50 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MW Uses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Teknor Apex Flexalloy® 9800-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Teknor Apex Flexalloy® 9800-60 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | |
AlphaGary Garaflex™ E 4762 A1 LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated low temperature flexible booster cable jacket application |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D-746 |
Axiall 18760 Wire & Cable Flexible PVC Non-lead stabilized, matte-finish, jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil. Ideally suited for 90°C applications.Information p.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746-98 |
Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where othe.. |
|||
Brittleness Temperature | -51.0 °C | -59.8 °F | ASTM D746 |
Eastman D4041-P Polyethylene
(discontinued **) Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an.. |
|||
Brittleness Temperature | -51.0 - -12.0 °C | -59.8 - 10.4 °F | Average value: -36.5 °C Grade Count:24 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |