Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -49.0 °C
-56.2 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable E1330I Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -49.0 °C
-56.2 °F
ASTM D746
PolyOne Elastamax™ HTE 3080 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..
Brittleness Temperature -49.0 °C
-56.2 °F
ASTM D746
Teknor Apex APEX® 2560-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Brittleness Temperature -49.0 °C
-56.2 °F
ASTM D746
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer
Notes: Non-halogenated; RoHS Compliant; MBDC: Green Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General ..
Brittleness Temperature -49.0 °C
-56.2 °F
ASTM D746
Colorite Polymers 6033 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Brittleness Temperature -49.0 °C
-56.2 °F
ASTM D746
Colorite Polymers 6034 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Brittleness Temperature -49.0 °C
-56.2 °F
AlphaGary Garaflex™ E 89-086 C3 NF LCF-R Vinyl Thermoplastic Elastomer
Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated flexible cord jacket compound