Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W9400 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W9400L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ HC 2185 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2185 is a 85 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2185 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ HC 2185G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2185G is a 85 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2185G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible D9002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -18.9 °C | -2.02 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R1765K Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |