Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJAX204V Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC340U Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 90072 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Eastman 812A Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Eastman 812P Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet... |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
Sylvin Technologies 6160-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 3310-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 3311-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 65002 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Lead-free Uses: Communication Wire JacketingForms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Ar.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex APEX® 84137 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Cable Jacketing Agency Ratings: UL 62 Wire Types: SAE; SJTW; SPT-1; SPT-2; SPT-3; SRDT; STW; SVTForms: PelletsIn.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Teknor Apex MF 573 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
Sylvin Technologies 6112-85 FU PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7009 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
AlphaGary Garaflex™ E X 05-384-G LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable60°C rated flexible compound for microphone & audio applications |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 10870 Wire & Cable Flexible PVC General purpose jacket compound recommended for 60C applications and also suited for 75C at a wall thickness of 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 18770 Moldings & Extrusions Flexible PVC General purpose 105C, clear jacketing compound recommended for 1/32" wall and larger. Exhibits excellent migration properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 18880 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated FT-4, tray cable jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 6850 Moldings & Extrusions Flexible PVC Low gravity compound for extrusion and molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
AlphaGary GW 2403-1 VW1 105-LCF Flame Retardant Polyvinyl Chloride 105°C rated low temperature oil & sunlight resistant jacketing compound for tray cable application |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 12870 Wire & Cable Flexible PVC 70°C oil, 80°C dry rated liquid tight conduit jacket meeting the requirements of UL 360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 16901 Wire & Cable Flexible PVC 90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 19802 Wire & Cable Flexible PVC Clear, 105°C rated extrusion compound recommended for 1/32" wall jacketing. Also well suited for injection molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Colorite Polymers 8002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 19801 Wire & Cable Flexible PVC Primary insulation and jacketing compound recommended for 105°C applications at a minimum wall of 15 mils. CSA approved AWM, SVT, SJT, ST, SVTO, SVTOO, SJTO, SJTOO, STO, STOO constructions. 60°C.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 22930 Coax & Telecom Flexible PVC Jacket compound suitable for riser applications when used with flame retardant PVC primaries. Maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 4441 Flexible PVC 85C non-lead stabilized wire harness. SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D-746 |
Axiall 83-126K Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | |
AlphaGary GW 2038 A VW1 LCF Flame Retardant Polyvinyl Chloride 60°C rated flame retarded jacketing compound for communications and riser cable applications |
|||
Brittleness Temperature | -28.0 °C | -18.4 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8050 Flexible PVC, Lead Free Pipes and profiles |