Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -26.1 °C | -15.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |
|||
Brittleness Temperature | -26.1 °C | -15.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -26.1 °C | -15.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R235AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -26.1 °C | -15.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R235AE White 1875 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -26.1 °C | -15.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R353AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -26.1 °C | -15.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |