Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 20 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 20 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required.Main Applications: Greenflex ML 20 is recommended for the production of flexible ite.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 21 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed.Main Applic.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: .. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex.. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746 |
ExxonMobil LL 5202.09 Compounding Resin
(discontinued **) LL 5202.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL 5202.09 makes for efficient blending with pigments, slip .. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Chevron Phillips Marlex® HMN 4550 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This resin is a high density polyethylene copolymer with high stress crack resistance, outstanding impact strength, and good warpage resistance. It is us.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Chevron Phillips Marlex® HMN 55180 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product disp.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D 746 |
Total Finathene® 6450 HDPE film
(discontinued **) Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin.. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
LG Chemical LUTENE-H XL1800 HDPE Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property an.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene EX1 is a high density polyethylene with 1-Butene as co monomer. It has acceptable tear strength, medium molar mass and narrow molar mass distribution.Applications: stretched film and tapes for prod.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr.. |
|||
Brittleness Temperature | >= -80.0 °C | >= -112 °F | ASTM D746-72 |
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending .. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746-95 |
Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation Description: Versilicâ„¢ SPX-70 I.B.: Produced form a proprietary combination of silicone elastomers, Versilicâ„¢ SPX-70 I.B. Tubing optimizes critical physical properties such as tensile st.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Brittleness Temperature | -80.0 °C | -112 °F | ASTM D746 |
DuPont™ Surlyn® 9650 Ionomer Resin, Zinc Surlyn® 9650 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Brittleness Temperature | -80.0 - -68.0 °C | -112 - -90.4 °F | Average value: -74.3 °C Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Brittleness Temperature | <= -80.0 °C | <= -112 °F | ASTM D746 |
LyondellBasell Alathon® 9301 High Density Polyethylene ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F.. |