Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -34.0 - -17.0 °C | -29.2 - 1.40 °F | Average value: -22.7 °C Grade Count:7 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |