Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= 0.000 °C | <= 32.0 °F | ASTM D746 |
Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection moldi.. |
|||
Brittleness Temperature | <= 0.000 °C | <= 32.0 °F | ASTM D746 |
Polimeri Europa Riblene® MV 10 R Low Density Polyethylene - Injection Molding Riblene MV 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 R are highly flexible.Main Applications: Riblene MV 10 R is ideal for injection.. |
|||
Brittleness Temperature | <= 0.000 °C | <= 32.0 °F | ASTM D746 |
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa. |
|||
Brittleness Temperature | 0.000 °C | 32.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | 0.000 °C | 32.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R148AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | 0.000 °C | 32.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R1700L Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | 0.000 °C | 32.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible F78E Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | 0.000 °C | 32.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R3578A Polyvinyl Chloride, Flexible (PVC, Flexible) A semirigid Vinyl Compound designed for edgeband applications with low migration characteristics.Information provided by PolyOne |
|||
Brittleness Temperature | >= 0.000 °C | >= 32.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Brittleness Temperature | >= 0.000 °C | >= 32.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Brittleness Temperature | >= 0.000 °C | >= 32.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Brittleness Temperature | 0.000 - 10.0 °C | 32.0 - 50.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Brittleness Temperature | 0.000 - 10.0 °C | 32.0 - 50.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Brittleness Temperature | 0.000 - 10.0 °C | 32.0 - 50.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Brittleness Temperature | 0.000 - 10.0 °C | 32.0 - 50.0 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Brittleness Temperature | 0.000 °C | 32.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R349AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |