Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC M40053S High Density Polyethylene for Injection Molding Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® GM 20 Low Density Polyethylene - Coating Grade Riblene GM 20 is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 20 is suitable for coating applications where a low neck-in is required. Moreover, for its rh.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polimeri Europa Riblene® GM 30 R Low Density Polyethylene - Coating Grade Riblene GM 30 R is a medium fluidity low density polyethylene resin (LDPE).Main Applications: Riblene GM 30 R is suitable for coating applications where low neck-in and high manufacturing speed are.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polymer Industries Densetec HDPE Pipe Grade The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It reta.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Polymer Industries Densetec HMW Sheet Polymer Industries’ Densetec HMW is the extruded material needed when Densetec HDPE is not enough and Polyslick UHMW™ is not necessary. Densetec HMW has higher impact strength than HDPE and is mor.. |
|||
Brittleness Temperature | -75.0 °C | -103 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D696 |
NOVA Chemicals Sclair® 51-35BP HDPE Extrusion Resin Features: Medium molecular weight, excellent ESCR, excellent toughness, good processability, good chemical resistance.Applications: Extrusion on to metal pipes to produce a corrosion resistant coati.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC BM1052 High Density Polyethylene for Blow Molding Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC M200024 Linear Low Density Polyethylene for Injection Molding Product Description: M200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give good f.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
SABIC M500026 Linear Low Density Polyethylene for Injection Molding Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos B35-150-134 MDPE
(discontinued **) Fortiflex® B35-150-134 is an intermediate density polyethylene copolymer developed for injection blow molding. It exhibits excellent gloss and environmental stress crack resistance (ESCR) in molde.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos G36-24-149 MDPE with Carbon Black
(discontinued **) Fortiflex® G36-24-149 is a black medium density polyethylene resin designed for sheet extrusion. This resin has excellent environmental stress crack resistance (ESCR) and ultra violet protection. .. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | F<SUB>50</SUB>; molding; ASTM D746 |
LyondellBasell Petrothene® NA942000 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone and agricultural and construction ma.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D 746 |
Ineos J50-200-178 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos T50-1000 HDPE Copolymer T50-1000 is a high density polyethylene copolymer. It has a narrow molecular weight distribution and provides injection molded parts with an excellent balance of properties and processing for most g.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos T50-500 HDPE Ineos T50-500 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and en.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos T60-500 HDPE T60-500 is a high density polyethylene homopolymer designed specifically for injection molding. This narrow molecular weight distribution resin is a product of Ineos USA, LLC's innovative technolog.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE F222 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
UBE F019 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A clamp, type 1 specimen; ASTM D746 |
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRBroad fusion rangeExcellent melt strengthGood processabilityExcellent flexibilityImproved output and texturingApplications: Coextruded ca.. |
|||
Brittleness Temperature | -75.0 °C | -103 °F | ASTM D746 |
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Brittleness Temperature | -75.0 - -70.0 °C | -103 - -94.0 °F | Average value: -70.6 °C Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Ineos HB111R Polyethylene Copolymer HB111R is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, particu.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A clamp, Type I Specimen; ASTM D746 |
Chevron Phillips Marlex® 9515H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, hexane copolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt str.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | ASTM D746 |
Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin
(discontinued **) Resin Type: Gas Phase Linear Hexene CopolymerASTM D 4976 Classification: PE 235, A 54607ASTM D3350 Classification: 335540AApplications: Base resin for use in utility and conduit pipe applications.Da.. |
|||
Brittleness Temperature | <= -75.0 °C | <= -103 °F | Type A, Type I specimen; ASTM D-746 |
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE High density polyethylene. This high molecular weight, hexene copolymer with synthetic antistatic agent is tailored for lightweight blow molded containers that: Require excellent stiffnessRequire .. |