Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® H&T CLH 150 Linear Low Density Polyethylene Clearflex H&T CLH 150 is a linear low density polyethylene resin, with antioxidants, suitable for cast film extrusion.Stretch films obtained from Clearflex H&T CLH 150 show good optical properties, .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D 746 |
Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled Information provided by PolyPlastic Group. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Flexirene® MS 20 U Linear Low Density Polyethylene Flexirene MS 20 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 U are characterized by optimum low tempe.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D 746 |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | F<sub>0</sub> notched specimen; ASTM D746 |
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, High Gloss, Excellent ImpactUses: Large houseware containers, General purpose injection molding |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
ExxonMobil Escorene® HD-6706 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Impact, Good Stiffness, Excellent ESCRUses: Pails, Industrial containers, Structural foams |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer The Tritheva® PN 2021 resin is an Ethylene-Vinyl Acetate copolymer (EVA) mainly used for the production of crosslinked/expanded plates and other parts. This is an easy processing product with high .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | ASTM D746 |
Lushan M-1 Adhesive Resin for Barrier Container and Tube Adhesive resin Lushan series for barrier container and tube is used for bonding a wide variety of materials, It’s most often used to adhering PE and EVOH, PP and EVOH, etc. Adhesive resins Lush.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Borealis Borecene™ RM7403 Linear Polyethylene for Rotational Molding Borecene Compact RM7403 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D696 |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | Average value: -70.0 °C Grade Count:9 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |
|||
Brittleness Temperature | -70.0 °C | -94.0 °F | DIN 53546 |
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Brittleness Temperature | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding.. |