Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -58.9 °C | -74.0 °F | ASTM D746 |
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Brittleness Temperature | -58.9 °C | -74.0 °F | ASTM D746 |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Brittleness Temperature | -58.9 °C | -74.0 °F | ASTM D746 |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |