Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Network Polymers Softflex® 6080 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3798 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
LyondellBasell Microthene® F FN50100 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D746 |
LG Chemical LUTENE XL2700BK PE Compound Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex APEX® 3201-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex APEX® 4150 Polyvinyl Chloride Compound Notes: Sunlight Resistant; 60°C Oil Resistant; Ultra Low Temperature Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex APEX® 65010 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-55-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1654A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-3050 Thermoplastic Elastomer Temperature Ratings: Wet Location: 75°C, Dry Location: 90°C Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | JIS K6301 |
Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ISO 974 |
Chengdu Polyster FH7560 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H7560 and self-made flame retardant material. Flame retardant, high tear resistance. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ISO 974 |
Chengdu Polyster H8570Y Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Low frictional coefficient and good abrasion resistance. Applications requiring high strength, high toughness .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 54 Flexible PVC, Injection Molding for Footwear Boots - sandshoes |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Colorite Polymers Weatherflex™ CS1536WX (NTL70B) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D-746 |
Axiall 16782 Wire & Cable Flexible PVC Non-lead stabilized, 90C jacketing compound with excellent low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D-746 |
Axiall 18754 Wire & Cable Flexible PVC Non-lead stabilized jacket compound with excellent low temperature performance. Maximum service temperature of 105°C at 40+ mil wall thickness.Information provided by Georgia GulfGeorgia Gulf beca.. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D726 |
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D746 |
Teknor Apex Elexar® EL-8730A Thermoplastic Elastomer Notes: Sunlight Resistant; Temperature Rating: 125°C Processing Method: Extrusion; Injection MoldingInformation Provided by Teknor Apex |