Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 90250 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -48.0 °C | <= -54.4 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **) A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Chevron Phillips 1006 LDPE Injection Molding Resin
(discontinued **) Resin Type: homopolymerCharacteristics: excellent flexibility, excellent flow, good warping resistance, moderate mold release, moderate ESCRApplications: large housewares, tamper evident snap-on cap.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | |
Sylvin Technologies 6404-78 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex APEX® 3201-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex APEX® 3301-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex APEX® 3311-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex Flexalloy® 9602-72FR Polyvinyl Chloride, Elastomer Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex APEX® 90-U656F1-72 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | <= -48.0 °C | <= -54.4 °F | ASTM D746 |
Teknor Apex Telcar® TL-1654B Thermoplastic Elastomer Notes: Non-halogenated Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstr.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ISO 974 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Colorite Polymers 8588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | |
Colorite Polymers Self Frosting™ 6011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D-746 |
Axiall EX1264 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for water stop applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D-746 |
Axiall 35061 Coax & Telecom Flexible PVC CMR jacket over PVC or flame retardant PE insulation with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D-746 |
Axiall 37740 Wire & Cable Flexible PVC 90°C rated compound designed for use as an inner and outer jacket in Teck 90 cables.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | |
AlphaGary PVC GSX 05-309 A2 UV Polyvinyl Chloride Thermoplastic Lead free flexible compound |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Colorite Polymers 6000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Teknor Apex APEX® 3050-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | |
Colorite Polymers 6011 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | |
Colorite Polymers 6012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable JG552NP Polyvinyl Chloride Alloy (PVC Alloy) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D746 |
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | |
AlphaGary GW 2326 A VW1 LCF Flame Retardant Polyvinyl Chloride 90°C rated low temperature jacket compound. |
|||
Brittleness Temperature | -48.0 °C | -54.4 °F | ASTM D-746 |
Axiall 38511 Wire & Cable Flexible PVC Tray cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |