Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable JLK51A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WA9001 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A9001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B90T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R291AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R356AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W2300 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |