Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ HC 2180G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180G is a 80 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2180G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 90215 Polyvinyl Chloride, Flexible (PVC, Flexible) Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible MD403KB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R293AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R3792E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D638 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 3611-90 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 89-P129A-NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: High Heat Resistant; Low to no Migration; Oil Resistant Uses: Flexible Cord Jacketing Agency Ratings: UL 62 Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 9300-85 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex HFFR 2004 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Uns.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-84 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7430 Flexible PVC, Injection Molding for Footwear Sandals |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 75/R1 Flexible PVC, Injection Molding for Footwear Soles antiaccident shoes |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7802 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Colorite Polymers 8566 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 7030 Flexible PVC, Extrusion Modified with Rubber Diesel Oil resistent profiles |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 65/AS Flexible PVC, Transparent Extrusion Food belt carriers |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PK 71/FR Flexible PVC, Lead Free Spiral pipes |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 7010 Flexible PVC, Extrusion Pipes and profiles |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 15881 Wire & Cable Flexible PVC 80C general purpose. 300 hour sunlight resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 17881 Wire & Cable Flexible PVC THW insulation compound. UL recognized component for TW, THW insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 16900 Wire & Cable Flexible PVC Tray cable jacket. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 19850 Moldings & Extrusions Flexible PVC Primary insulation compound recommended for 105C, 1/32 wall and larger applications. Also well suited for plug molding. UL rated 94 HB.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 19854 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound. Recognized by UL for TW and THW applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 19880 Wire & Cable Flexible PVC 105°C rated, 30 mil and larger, clear compound recommended for VW-1 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
AlphaGary PVC GM 5075 Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 6805 Flexible PVC, Lead Free Various profiles |