Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 1800-xx19D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx17FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable EMB405L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC330 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746-98 |
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
S&E Specialty Polymers TufTech™ GA-3188AHP PVC Compound Application: RoHS compliant, phthalate free, 105°C flame retardant jacketing material suitable for extrusion applications.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | <= -20.0 °C | <= -4.00 °F | ASTM D746 |
Polimeri Europa Riblene® MR 10 R Low Density Polyethylene - Injection Molding Riblene MR 10 R is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 R are characterized by a high flexibility.Main Applications: Riblene MR 10 R is suitable for i.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible P484 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R111AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R2495A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3437 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible P484B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -20.0 °C | <= -4.00 °F | ASTM D 746 |
Karina 937-48/1-CY-IS-BZ Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 2090-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 3200-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 96-A0914M-90 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant Uses: Communication Wire Jacketing Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 820; UL 1424; UL 444; UL 62 Wire Types: FT-4; MPR For.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 1011 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7516 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS6037GP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow 959S Linear Low Density Polyethylene (LDPE) DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 86/AF Flexible PVC, Extrusion Modified with Rubber Profiels UL 94 Classe V0 |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 21571 Coax & Telecom Flexible PVC Semi-rigid insulation compound designed for data communication riser cable application.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
AlphaGary GW 2403-1 VW1 75 LCF Flame Retardant Polyvinyl Chloride 75°C rated jacket compound |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1201 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8220 Flexible PVC, Lead Free Various profiles |