Polymer Property : Brittleness Temperature = -18.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W9400 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W9400L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ HC 2185 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2185 is a 85 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2185 can be used for extrusion and injection molding healthcare applications.NOTE: All ing..
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ HC 2185G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2185G is a 85 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2185G can be used for extrusion and injection molding healthcare applicatio..
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible D9002 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -18.9 °C
-2.02 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R1765K Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne