Polymer Property : Brittleness Temperature = -13.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -13.0 °C
8.60 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W1349L NAT 0000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Brittleness Temperature -13.0 °C
8.60 °F
ASTM D746
Teknor Apex APEX® 80873 Polyvinyl Chloride, Semi-Rigid
Notes: 105°C Insulation; RoHS Compliant Features: Semi-rigid Uses: Insulation; Automotive Electronics Agency Ratings: UL 1063; UL 1581; UL 83; SAE J1128 Forms: Pellets Wire Types: THHN; THW; TW; ..
Brittleness Temperature -13.0 °C
8.60 °F
Cold Flex; ISO 458/2
Fainplast Compounds PM 9012 Flexible PVC, Extrusion
Furniture border
Brittleness Temperature -13.0 °C
8.60 °F
ASTM D746
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -13.0 °C
8.60 °F
ASTM D746
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -13.0 °C
8.60 °F
AlphaGary Smokeguard™ HP 505 High Performance Fluoropolymer
Smokeguard™ HP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements
Brittleness Temperature -13.0 °C
8.60 °F
AlphaGary GW 3010 LCF P Flame Retardant Polyvinyl Chloride
60°C or 75°C rated jacket compound.
Brittleness Temperature -13.0 °C
8.60 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W1349L-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..