Thermal Properties | Metric | English | Comments |
---|---|---|---|
Distillation Temperature | 222 - 224 °C | 432 - 435 °F | |
Solvay RHODISOLV® IRIS Solvent Description: Rhodiasolv IRIS is a new biodegradable, eco-friendly, non flammable and non VOC solvent.Identification: DIMETHYL 2-METHYLGLUTARATECAS: 14035 – 94 – 0ELINCS: 486 – 070 – 7Available i.. |